MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultradur® B 4040 G10 High Speed BK15029 50% Glass Filled PBT/PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled; Polyethylene Terephthalate (PET)

Material Notes: Ultradur B 4040 G10 High Speed BK15029 is a high flow, fast cycling with low warpage, 50% glass filled, injection molding PBT for industrial parts, rigid tough and dimensional stable applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.76 g/ccISO 1183
Water Absorption 0.40 %ISO 62
Moisture Absorption at Equilibrium 0.12 %23°C/50% R.H.; ISO 62
Viscosity Number 75 cm³/g
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO Data
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO Data
Melt Flow 130 g/10 min
@Load 2.16 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 150 MPa5mm/min; ISO 527
Elongation at Break 1.2 %5mm/min; ISO 527
Tensile Modulus 18400 MPa1mm/min; ISO 527
Charpy Impact, Notched 1.00 J/cm²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 4.5
@Frequency 1e+6 Hz
IEC 60250
 4.7
@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0020
@Frequency 100 Hz
IEC 60250
 0.015
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 225 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.0 µm/m-°CISO 11359
Melting Point 223 °C10 K/min
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75
 
Descriptive Properties
ColorBK15029
Commercial StatusNorth America and Europe
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultradur® B 4040 G10 LS High Speed BK15029 50% Glass Filled PBT/PET
BASF Ultradur® B 4040 G4 LS High Speed BK15029 20% Glass Filled PBT/PET
BASF Ultradur® B 4040 G6 High Speed BK15029 30% Glass Filled PBT/PET
BASF Ultradur® B 4040 G6 LS High Speed BK15029 30% Glass Filled PBT/PET
BASF Ultradur® B 4040 G10 BK5110 50% Glass Filled PBT

PBASF9059 / 84823

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.