MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Reaction Bonded Silicon Nitride Mac-RBSNS Technical Ceramic
Categories: Ceramic; Nitride

Material Notes: An advanced synthetic ceramic. Reaction bonded silicon nitride (RSBN) is made by directly reacting compacted silicon powder with nitrogen to produce porous components of relatively low density and possessing exceptional thermal.

Applications:

  • Welding jigs and fixtures
  • Molten non-ferrous metal handling systems
  • Riser tubes and transfer tubes
  • Delivery systems and degassing systems
  • Special crucibles

information provided by Morgan Advanced Materials

Key Words: Technical Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.50 g/ccfired
Porosity 20 %nominal
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 170 GPa
@Temperature 20.0 °C
Flexural Strength 200 MPa
@Temperature 20.0 °C
3-point
Compressive Strength 650 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1.00e+10 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.10 µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 1.10 J/g-°C
Thermal Conductivity 12.0 W/m-K
@Temperature 20.0 °C
Maximum Service Temperature, Air 1300 °CNo-Load
 
Component Elements PropertiesOriginal ValueComments
Si3N4 99 %
 
Descriptive Properties
Colorgray
Thermal Downshock>600sC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Techical Ceramics Ekasic® S Silicon Nitride
3M Techical Ceramics Ekatherm® Silicon Nitride
3M Techical Ceramics Ekasic® T Plus Silicon Carbide
3M Techical Ceramics Ekasic® P Silicon Carbide
3M Techical Ceramics Ekasic® G Silicon Carbide

CMORF8046 / 203523

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.