MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy; <25 mm
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: High-Strength Forging Alloy

Industry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.

Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a similar composition to TIMETAL 550, apart from an increase in tin content, which gives increased strength at room and elevated temperatures. This is one of the strongest of the commercially available titanium alloys, with room temperature strengths ranging form 1250 to 1400 MPa. Typical applications include airframe structural forgings and machined parts such as undercarriage components, mounting brackets and pump casing where strength is required at low weight; and gas-turbine engine components. The alloy is also suitable for general engineering applications such as steam-turbine blades, axial and radial compressor parts, connecting rods, and other high-speed rotating and reciprocating components. It is nonmagnetic.

Typical heat treatment for this alloy: Solution heat treatment: 900°C for 1 hr, air cool. Ageing heat treatment: 500°C for 24 hrs, air cool.

Data provided by TIMET.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 4.60 g/ccTypical
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1450 MPaTypical
Tensile Strength, Yield 1210 MPa
@Strain 0.2 %
Typical
Elongation at Break 10 %Typical
Reduction of Area 20 %
Modulus of Elasticity 110 - 120 GPaTypical
Poissons Ratio 0.34Calculated by MatWeb
Fatigue Strength 400 MPa
@# of Cycles 1.00e+8
Notched, Kt = 3.2; 1" (25 mm) diameter rod
 790 MPa
@Diameter 25.0 mm,
# of Cycles 1.00e+8
smooth, rod
Fracture Toughness 30.7 MPa-m½K(IC)
Shear Modulus 43.0 GPa
Charpy Impact 25.0 Jat RT
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000170 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.50 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.368 J/g-°C
Thermal Conductivity 6.92 W/m-K
Maximum Service Temperature, Air 400 °CUseful creep to 400°C
Beta Transus 1050 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 3.0 - 5.0 %
Carbon, C 0.050 - 0.20 %
Hydrogen, H <= 0.015 %
Iron, Fe <= 0.20 %
Molybdenum, Mo 3.0 - 5.0 %
Nitrogen, N <= 0.050 %
Oxygen, O <= 0.25 %
Silicon, Si 0.30 - 0.70 %
Tin, Sn 3.0 - 5.0 %
Titanium, Ti 83.2 - 90.7 %Calculated as remainder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); 40% Cold Work
Titanium Ti-15Mo-5Zr ST 730°C, Aged 400°C
Special Metals Nitinol Chrome-Doped Superelastic Ni-Ti alloy
Special Metals Nitinol High-Strength Superelastic Ni-Ti alloy
Special Metals Nitinol High-Strength Superelastic Ni-Ti-Fe alloy

NTIME551 / 19305

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.