MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Taro Plast Taroblend 70 PC/PBT
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: PC/PBT alloy, good impact strength combined with good chemical resistance. Available: all colors, UV stabilized (L).

Information provided by Taro Plast S.p.a.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ISO 1183
Water Absorption 0.090 %
@Time 86400 sec
0.090 %
@Time 24.0 hour
ISO 62
Water Absorption at Saturation 0.45 %0.45 %ISO 62
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm0.010 - 0.012 in/inISO 2577
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm0.010 - 0.012 in/inISO 2577
Melt Flow 35 g/10 min
@Load 5.00 kg,
Temperature 260 °C
35 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.0 MPa7980 psiISO 527
Tensile Strength, Yield 60.0 MPa8700 psiISO 527
Elongation at Break >= 100 %>= 100 %ISO 527
Tensile Modulus 2.30 GPa334 ksiISO 527
Flexural Strength 95.0 MPa13800 psiISO 178
Flexural Modulus 2.10 GPa305 ksiISO 178
Izod Impact, Notched 0.800 J/cm1.50 ft-lb/in127x12.7x3.2; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 300 V300 VMethod A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C
@Time 72000 sec
212 °F
@Time 20.0 hour
IEC 60216
Hot Ball Pressure Test 145 °C293 °FIEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FISO 75/A
Vicat Softening Point 180 °C
@Load 1.00 kg
356 °F
@Load 2.20 lb
ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
127x2.17xThickness
Glow Wire Flammability Index 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
60x60xThickness; IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTARO112 / 283220

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.