Description: TIPPLEN H 649 FH is a homopolymer polypropylene for the production of biaxially oriented films. The grade contains reinforced processing stabilization but does not contain any slip or antiblocking agents. Applications: TIPPLEN H 649 FH is Ca-stearate free and it is particularly suitable for metallization both in monolayer and in coextruded structures. TIPPLEN H 649 FH has good mechanical properties, high impact strength and puncture resistance even at low temperatures. The BOPP film forms an excellent barrier against moisture, oils and oxidation and features good optical properties. Monolayer or coextruded films with a thickness range of 0.01 – 0.04 mm are used for packaging. (1) Average mechanical property values of several measurements carried out on standard injection-molded test specimens prepared in accordance with ISO 294-1. Information provided by Molgroup Chemicals |