The Nymax® Series of nylon 6/6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of fillers, glass reinforcement levels, and impact modifiers depending upon grade selected and have been formulated to offer ease of processing in most standard thermoplastic processing equipment. Description/Features: - Nylon 6/6 Compound
- Impact Modified
- Black
Applications: Market: - Automotive
- Building and Construction
- Industrial
- Consumer Goods
Processing Method: Molded Test Bars: (Dry as Molded;PolyOne First Choice Information provided by PolyOne Corporation. |