MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Morgan Advanced Ceramics Encast LI Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Chamotte raw material base. Hydraulic bond. Low iron, high duty, general purpose castable. Applications: Heat containment applications up to 1500°C requiring low iron and good thermal shock resistance.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.08 g/cc0.0751 lb/in³dried to 110°C
Grain Size <= 6000 µm<= 6000 µm
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength  12.0 MPa
@Treatment Temp. 1000 °C
1740 psi
@Treatment Temp. 1830 °F
Cold Crushing Strength
 16.0 MPa
@Treatment Temp. 815 °C
2320 psi
@Treatment Temp. 1500 °F
Cold Crushing Strength
 21.0 MPa
@Treatment Temp. 110 °C
3050 psi
@Treatment Temp. 230 °F
Cold Crushing Strength
 42.0 MPa
@Treatment Temp. 1500 °C
6090 psi
@Treatment Temp. 2730 °F
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.790 W/m-K
@Temperature 600 °C
5.48 BTU-in/hr-ft²-°F
@Temperature 1110 °F
Maximum Service Temperature, Air <= 1500 °C<= 2730 °F
Shrinkage  -0.500 - 0.50 %
@Treatment Temp. 1500 °C
-0.500 - 0.50 %
@Treatment Temp. 2730 °F
 0.00 - 0.20 %
@Treatment Temp. 110 °C
0.00 - 0.20 %
@Treatment Temp. 230 °F
 0.10 %
@Treatment Temp. 815 °C
0.10 %
@Treatment Temp. 1500 °F
 0.30 %
@Treatment Temp. 1000 °C
0.30 %
@Treatment Temp. 1830 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 47 %47 %
CaO 6.0 %6.0 %
Fe2O3 1.0 %1.0 %
SiO2 43 %43 %
 
Descriptive Properties
Net Material Required (kg/m³)2060
Water Addition11-13 % by weight, 2.75-3.25 L bag, 25 kg bag weight.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6255 / 203039

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.