MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SK Chemicals SARAN™ 540-CX Vapor Retarder Tape  (discontinued **)
Categories: Polymer; Adhesive

Material Notes: SARAN™ 540-CX Vapor Retarder Film is composed of a film of the barrier polymer polyvinylidene chloride (PVDC) coextruded with other specialty polymers that provide strength and support. Working together, the portions of this coextruded film combine to create a vapor retarder and jacketing material for mechanical insulation systems that is durable, flexible and has excellent resistance to water vapor penetration. SARAN 540-CX Film is designed specifically to help prevent water absorption and strongly resist moisture vapor drive into the insulation. A permeance rating of 0.02 perms meets or exceeds standard industry requirements for vapor retarders in cold service. SARAN 540-CX Vapor Retarder Film is not a known nutrient source for mold or mildew.

Applications: SARAN 540-CX Vapor Retarder Film is a high-performance, cost effective vapor retarder used in many pipe insulation applications. Typical applications for SARAN 540 CX Film include:

  • Food and beverage facilities
  • Chilled water piping and HVAC systems
  • Transport pipelines
  • Chemical condensation tanks
  • Cold storage systems
  • Refrigerated transport
  • Pharmaceutical plants
  • Petrochemical plants

SK Global Chemical has purchased the SARAN® resin business from Dow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Vapor Transmission 1.01 g/m²/day
@Temperature 37.8 °C
0.0650 g/100 in²/day
@Temperature 100 °F
90% RH; ASTM F1249
Thickness 102 microns4.00 milASTM D374
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 14.8 MPa2150 psiUltimate; ASTM D882
Film Tensile Strength at Yield, TD 13.0 MPa1890 psiUltimate; ASTM D882
Film Elongation at Yield, MD 291 %291 %Ultimate; ASTM D882
Film Elongation at Yield, TD 242 %242 %Ultimate; ASTM D882
2% Secant Modulus 0.494 GPa71.7 ksiMD; ASTM D822
 0.498 GPa72.3 ksiTD; ASTM D822
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flame Spread Index 1010ASTM E84
Shrinkage  >= 1.0 %
@Temperature 100 °C
>= 1.0 %
@Temperature 212 °F
Unrestrained, Air, MD
 >= 1.0 %
@Temperature 100 °C
>= 1.0 %
@Temperature 212 °F
Unrestrained, Air, TD
 
Descriptive Properties
ColorWhite
Mullen Burst Strength75 lbs/in²ASTM D774
Permeance0.02ASTM E96
Surface Burning Characteristics20Smoke Developed, ASTM E84
Ultimate Tensile Strength8 lb/inwidth, TD, ASTM D882
 9 lb/inwidth, MD, ASTM D882
Yield39.2 ft²/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tin, Sn
SK Chemicals Saran® 313 PVDC
Water, H2O
Morgan Advanced Ceramics Pyrolytic Boron Nitride PBN Chemical Vapor Deposition Ceramic
SK Chemicals SARAN™ 560-CX Vapor Retarder Film

PITWZ002 / 187068

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.