System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Mytex Polymers AN16L(W)-D56 Polypropylene, Talc filled, Compounded, Elastomer, Impact modified
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 10% Talc Filler
Material Notes:
Description: AN16L-D56 is a compounded talc filled elastomer modified polypropylene with good impact and excellent material flow properties.
Key Applications: Automotive exterior
Information provided by Mytex Polymers
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.930
g/cc
ASTM D792
Melt Flow
17
g/10 min
ASTM D1238
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
105
MPa
50 mm/min; ASTM D638
Tensile Strength, Yield
19.0
MPa
50 mm/min; ASTM D638
Flexural Strength
23.0
MPa
Max load; 1.3 mm/min; ASTM D790
Flexural Modulus
1150
MPa
Tangent; 1.3 mm/min; ASTM D790
Izod Impact, Notched
450
J/m
@Temperature 23.0 °C
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
85.0
°C
ASTM D648
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Mytex Polymers AS23KW-01 Polypropylene, Talc filled, Compounded
A. Schulman TPP20AF01HB 20% Talc-Filled Homopolymer Polypropylene
Overview of materials for Polypropylene with 10% Mica Filler
Overview of materials for Polypropylene with 10% Talc Filler
Overview of materials for Polypropylene with 20% Mica Filler
PMYTEX003 / 90293
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.