MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lion SBR 1783L Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: SBR 1783L is an environmentally friendly version of SBR 1712 replacing aromatic extender oil with a 37.5 parts of low Polycyclic Aromatic Hydrocarbon RAE oil. It was developed for tire applications.

Unique Features:

  • Cold polymerized styrene-butadiene elastomer
  • Lower Mooney viscosity & RAE oil extended
Applications:
  • Passenger & heavy-service treads
  • Retread rubbers and bicycle tires

Information provided by Lion Elastomer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.950 g/cc0.950 g/cc
Volatiles <= 0.75 %<= 0.75 %ASTM D5668
Mooney Viscosity 40 - 50
@Temperature 100 °C
40 - 50
@Temperature 212 °F
ML (1+4); ASTM D 1646
Ash <= 0.80 %<= 0.80 %ASTM D5667
 
Chemical PropertiesMetricEnglishComments
Styrene Content 22.5 - 24.5 %22.5 - 24.5 %Bound; ASTM D5775
 
Descriptive Properties
Content<0.5%Soap, ASTM D5774
 4-6%Organic acid, ASTM D5774
Oil25.8-28.8%Oil, ASTM D5774

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLION036 / 317945

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.