MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lord Adhesives Chemlok® 8007 Blue Primer
Categories: Polymer; Adhesive

Material Notes: LORD Chemlok® 8007 Blue aqueous (water-based) primer is designed to bond elastomers to metals and other substrates when used with Chemlok water-based covercoat adhesives, including Chemlok 8560S, Chemlok 8560D and Chemlok 8210 adhesives. It is composed of a mixture of dispersed mineral fillers, organic compounds, resins and polymer lattices in an water-based medium.

Features: provides reduced VOC emissions, allowing for a safer work environment. functions as an effective primer for many materials such as steel, phosphated steel, nylon, aluminum and brass. provides excellent resistance to water, salt spray, glycol, oil and heat. provides a smooth coating for use by dip or spray applications. The blue color affords good contrast with black covercoats and prepared metals. easily redispersed within 5 to 15 minutes of stirring; ready to use directly out of the container without dilution.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 - 1.17 g/cc0.0407 - 0.0424 lb/in³
Solids Content 29 - 33 %29 - 33 %by weight
Brookfield Viscosity 15 - 250 cP
@Temperature 25.0 °C
15 - 250 cP
@Temperature 77.0 °F
Brookfield LVT, Spindle 2, 30 rpm
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 93.0 °C>= 199 °FSeta
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month
@Temperature 21.0 - 27.0 °C
3.00 Month
@Temperature 69.8 - 80.6 °F
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceBlue liquid
pH6 to 8
SolventsDeionized Water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9060 / 232449

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.