MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Carpenter Extendo-Die® Hot Work Die Steel, Tempered 621°C
Categories: Metal; Ferrous Metal; Tool Steel; Air-Hardening Steel; Hot Work Steel

Material Notes: Data provided by Carpenter Technology Corporation.

This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applications where H13 is used, particularly in large section size applications. Extendo-Die® hot work die steel can be water cooled in service.

Extendo-Die® is a registered trademark of Carpenter Technology Corporation.

Key Words: UNS K92580
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.72 g/cc0.279 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 395395Estimated from Rockwell C for 3000 kg load, 10 mm ball Brinell measurement.
Hardness, Knoop 431431Estimated from Rockwell C
Hardness, Rockwell C 42.542.5
Hardness, Vickers 413413Estimated from Rockwell C
Tensile Strength, Ultimate 1450 MPa210000 psi
Tensile Strength, Yield 1200 MPa
@Strain 0.2 %
174000 psi
@Strain 0.2 %
Elongation at Break 12 %12 %
Reduction of Area 40 %40 %
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.6 µm/m-°C
@Temperature 24.0 - 93.0 °C
5.89 µin/in-°F
@Temperature 75.2 - 199 °F
 12.6 µm/m-°C
@Temperature 427 - 788 °C
7.00 µin/in-°F
@Temperature 801 - 1450 °F
 13.1 µm/m-°C
@Temperature 24.0 - 649 °C
7.28 µin/in-°F
@Temperature 75.2 - 1200 °F
Transformation Temperature 857 °C1570 °FAc1
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.44 %0.44 %
Chromium, Cr 6.0 %6.0 %
Iron, Fe 89 %89 %as remainder
Manganese, Mn 0.45 %0.45 %
Molybdenum, Mo 1.9 %1.9 %
Silicon, Si 1.0 %1.0 %
Sulfur, S <= 0.0050 %<= 0.0050 %
Vanadium, V 0.80 %0.80 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type 316F Stainless Steel, annealed bar
AISI Type 430F Stainless Steel annealed bar
AISI Type P4 Mold Steel, air cooled from 955°C, tempered at 425°C
Overview of materials for Air-Hardening Steel
Schmolz + Bickenbach 416 Stainless Steel Bar

NCARM2 / 15837

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.