MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SunChemical Gwent C60531D1 Silver / Silver Chloride Paste
Categories: Fluid; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: C60531D1 has a ratio of Silver to Silver Chloride of 90/10. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a family of reference electrode materials with ratios from 40/60 through 90/10 Silver/Silver Chloride.

The paste is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The paste should be gently stirred before use avoiding introduction of air bubbles. It is a Polymer System for printing on polyester, PVC, Polycarbonate etc and on alumina.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 3500 - 7000 cP3500 - 7000 cP
 3900 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
3900 cP
@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake Viscosity
Thickness 17.0 microns0.669 milwhen printed through a 156 mesh
Storage Temperature 20.0 °C68.0 °Fin a sealed pot
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 0.20 ohm0.20 ohmcured film; 17 microns thick
 
Processing PropertiesMetricEnglishComments
Cure Time  10.0 min
@Temperature 80.0 °C
0.167 hour
@Temperature 176 °F
 30.0 min
@Temperature 60.0 °C
0.500 hour
@Temperature 140 °F
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
Conductive Filler TypeSilver (Ag) / Silver Chloride (AgCl)
Coverage cm2/g185156 mesh polyester mesh screen with 13 micron emulsion back off
Material TypeReady-To-Use Formulation
Printing Mesh counts/inch120 to 200typical screen size is 156 Polyester
Recommended SubstratesPolyester, PVC, Polycarbonate or Ceramic
Solvent SystemEthoxy Propanol or Sericol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SunChemical Gwent C2030701P1 Silver/Silver Chloride Paste

WGEM043 / 75896

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.