System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Omni Plastics OmniLon™ PA6/6 GR35 NHFR0 HS Nylon 6/6, 35% Glass reinforced
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 40% Glass Fiber Filled
Material Notes:
35% Glass reinforced, chlorine and bromine free, flame resistant, heat stabilized; values are based on natural or black materials unless otherwise noted.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.44
g/cc
ASTM D792
Filler Content
35 %
ASTM D2584
Linear Mold Shrinkage
0.0010
-
0.0040
in/in
ASTM D955
Linear Mold Shrinkage, Transverse
0.0040
-
0.0080
in/in
ASTM D955
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
172
MPa
ASTM D638
Elongation at Break
2.0 %
ASTM D638
Flexural Strength
293
MPa
ASTM D790
Flexural Modulus
10342
MPa
ASTM D790
Izod Impact, Notched
96.0
J/m
@Thickness 3.17 mm
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
257
°C
@Thickness 3.17 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
243
°C
@Thickness 3.17 mm
ASTM D648
Flammability, UL94
V-0
@Thickness 3.00 mm
Black Color Only
V-0
@Thickness 1.50 mm
Black Color Only
Processing Properties
Original Value
Comments
Rear Barrel Temperature
520
-
560
°F
Middle Barrel Temperature
520
-
560
°F
Front Barrel Temperature
520
-
560
°F
Nozzle Temperature
520
-
560
°F
Melt Temperature
520
-
560
°F
Mold Temperature
80.0
-
140
°F
Drying Temperature
180
°F
Dry Time
2.00
-
4.00
hour
Moisture Content
<= 0.20 %
Back Pressure
50.0
psi
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Envalior Akulon® K224-G7 PA6-GF35, Dry, 35% Glass Filled
Envalior Akulon® Ultraflow K-FHG8 PA6-GF40, Dry, 40% Glass Filled, Heat Stabilized
Envalior Akulon® K224-HGM35 PA6-(GF+MD)40, Conditioned, 15/25% Glass/Mineral Filled, Heat Stabilized
Envalior Akulon® K224-HG7 PA6-GF35, Dry, 35% Glass Filled, Heat Stabilized
Envalior Akulon® K224-G7 PA6-GF35, Conditioned, 35% Glass Filled
POMNI5015 / 185161
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.