MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röchling Polystone® M Reprocessed UHMW-PE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes:
  • High abrasion and wear resistance
  • Low coefficient of friction
  • Economical grade
Product applications:
  • Wear strips
  • Chute and hopper liners
  • Chain guides

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 - 0.940 g/cc0.0336 - 0.0340 lb/in³ASTM D792
Water Absorption <= 0.010 %<= 0.010 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 63 - 6963 - 69ASTM D2240
Tensile Strength, Yield 20.7 MPa3000 psiASTM D638
Elongation at Break >= 290 %>= 290 %ASTM D638
Tensile Modulus 0.689 GPa100 ksiASTM D638
Flexural Strength 19.3 MPa2800 psiASTM D790
Izod Impact, Notched NBNBASTM D638
Izod Impact, Notched (ISO) 96.0 kJ/m²45.7 ft-lb/in²ASTM D4020
Coefficient of Friction, Dynamic 0.10 - 0.220.10 - 0.22Dry vs. Steel
Coefficient of Friction, Static 0.15 - 0.250.15 - 0.25Dry vs. Steel
Sand Slurry 9090
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+12 ohm>= 1.00e+12 ohmASTM D257
 >= 1.00e+15 ohm>= 1.00e+15 ohmASTM D257
Dielectric Constant 2.3
@Frequency 1e+6 Hz
2.3
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 45.0 kV/mm1140 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 198 µm/m-°C110 µin/in-°FASTM D696
Melting Point 130 - 135 °C266 - 275 °F
Maximum Service Temperature, Air 82.2 °C180 °F
Deflection Temperature at 1.8 MPa (264 psi) 46.7 °C116 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Compliance PropertiesMetricEnglishComments
FDA NoNo
NSF NoNo
USDA NoNo
 
Descriptive Properties
ColorBlack, Green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman tetra-DUR F 4401 Bulk Molding Compound
Röchling Polystone® M XL Cross linked UHMW-PE
Röchling Polystone® M Virgin UHMW-PE
Röchling Polystone® M MPG Glass filled UHMW-PE
Röchling Polystone® G Black Utility HDPE

PROCH006 / 66210

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.