MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Avient Elastamax™ HTE 1102 Styrene Butadiene Block Copolymer (SBC)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.918 g/cc0.918 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm0.018 - 0.020 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4747ASTM D2240
Tensile Strength at Break 3.79 - 4.14 MPa550 - 600 psi510 mm/min; ASTM D412A
Elongation at Break 900 %900 %510 mm/min; ASTM D412A
Tear Strength 19.8 kN/m113 pliDie C, 510 mm/min; ASTM D624
 
Descriptive Properties
FeaturesGeneral Purpose
FormsPellets
Generic MaterialSBC
Generic NameStyrene Butadiene Block Copolymer (SBC)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Interior Parts
 Consumer Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Elastamax™ HTE 1105 Styrene Butadiene Block Copolymer (SBC)
Avient Elastamax™ HTE 1104 Styrene Butadiene Block Copolymer (SBC)
Avient Elastamax™ HTE 1101 Styrene Butadiene Block Copolymer (SBC)
Celanese SO.F.TER Sofprene T® 5405.A50 SBS TPE
Kraton® D2109 DS-N (SBS) Compound

PH0POL0453 / 145022

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.