MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
EOS CobaltChrome MP1 DMSL on EOS M 100; 30 µm Layer Thickness
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Cobalt Alloy

Material Notes: EOS CoCr MP1 conforms to chemical composition UNS R31538. Parts built can be machined, welded, polished and coated as required. They are suitable for a wide variety of applications.

Main Characteristics:

  • High carbon CoCrMo based superalloy
  • Good corrosion and wear resistance
  • Good mechanical properties
Typical Applications:
  • Orthopedic implants
  • Gas turbines
  • Engine components
  • Jewelry

Information provided by EOS GmbH (Electro Optical Systems).

Key Words: UNS R31538
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Porosity <= 0.20 %
Thickness 30.0 microns
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 830 MPaVertical
 1040 MPaHorizontal
Tensile Strength, Yield 1200 MPaVertical
 1340 MPaHorizontal
Elongation at Break 11 %Horizontal
 13 %Vertical
 
Descriptive Properties
Volume rate1.5 mm3/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NEOS923 / 280583

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.