MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 2582 HEC FR Polycarbonate/ABS Alloy (PC/ABS) Nickel-Coated Carbon Fiber - EMI/RFI Shielding - Electrically Conductive - Flame Retardant - UL94 V-0
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, NCG Fiber Filled; Polycarbonate (PC)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.37 g/ccASTM D 792
Additive Loading 15 %Primary Additive
Linear Mold Shrinkage 0.00050 - 0.0025 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 16400 psiASTM D 638
Elongation at Break 1.0 - 2.0 %ASTM D 638
Tensile Modulus 1200 ksiASTM D 638
Flexural Strength 22000 psiASTM D 790
Flexural Modulus 1200 ksiASTM D 790
Izod Impact, Notched 0.700 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 5.80 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 10 ohm-cmASTM D 257
Surface Resistance <= 1000 ohmESD STM11.11
Surface Resistivity per Square <= 10000 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness 73 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 80 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 81 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
ASTM D 4935
 87 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 88 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
ASTM D 4935
 95 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 95 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 100 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 100 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 101 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 102 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 105 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
@Thickness 1.50 mm
 5VA
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 470 - 525 °F
Mold Temperature 125 - 200 °F
Drying Temperature 200 °F
@Time 14400 sec
Moisture Content 0.020 %
Dew Point -20.0 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo PULSE™ 2000 EZ PC/ABS Engineering Resin
Mitsubishi Iupilon® EHR 3400 Polycarbonate
Covestro Makrolon® GF9002 Polycarbonate, 10% Glass Filled

PQZWA2518 / 91196

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.