MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Cast Nylons Nycast® 12 Cast Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Cast

Material Notes: NYCAST® 12 is specially formulated and designed to offer very low moisture absorption, superior wear resistance, dimensional stability, exceptional lubrication ability, outstanding mechanical characteristics, high impact strength, and lower thermal expansion. Typical applications include wheels, rollers, bearings & bushings, gears, and valve seals.

Data provided by the manufacturer, Cast Nylons Limited.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ASTM D792
Water Absorption 0.12 %0.12 %24 hrs; ASTM D570
Water Absorption at Saturation 0.66 %0.66 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 108108ASTM D785
Hardness, Shore D 7676ASTM D2240
Tensile Strength 54.5 MPa7900 psiASTM D638
Elongation at Break >= 50 %>= 50 %ASTM D638
Tensile Modulus 1.59 GPa230 ksiASTM D638
Flexural Strength 62.1 MPa9000 psiASTM D790
Flexural Modulus 1.64 GPa238 ksiASTM D790
Compressive Strength 68.9 MPa10000 psiASTM D695
Compressive Modulus 1.54 GPa224 ksiASTM D695
Shear Strength 42.1 MPa6100 psiASTM D732
Izod Impact, Notched 1.61 J/cm3.02 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.2 - 0.30.2 - 0.3ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.7
@Frequency 60 Hz
3.7
@Frequency 60 Hz
ASTM D150
 3.7
@Frequency 1000 Hz
3.7
@Frequency 1000 Hz
ASTM D150
 3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 19.7 - 23.6 kV/mm500 - 600 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 99.0 µm/m-°C55.0 µin/in-°FASTM D696
Melting Point 177 °C351 °FASTM D789
Maximum Service Temperature, Air 121 °C250 °FContinuous
 149 °C300 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 175 °C347 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C124 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema ORGASOL® 2002 D Nat 1 Polyamide 12, Food Contact Approved
Overview of materials for Nylon 12
Cast Nylons Nycast® GX Solid Lubricant Filled Gray Cast Nylon 6
Arkema ORGASOL® 2001 UD Nat 2 Polyamide 12, Food Contact Approved
Arkema ORGASOL® 2001 EXD Nat 1 Polyamide 12, Food Contact Approved

PCAST99 / 149808

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.