MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 4.0 PHR Di-Cup 40C Peroxide
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.

Curing of Millathane®76 can easily be done with many types of peroxides. Millathane76 peroxide vulcanizates have superior compression set, greater heat stability, and are more resistant to reversion than sulfur cures..

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6868
Tensile Strength 30.23 MPa4384 psi
Elongation at Break 277 %277 %
100% Modulus 4.66 MPa
@Strain 100 %
676 psi
@Strain 100 %
200% Modulus 17.26 MPa
@Strain 200 %
2504 psi
@Strain 200 %
Tear Strength 59.7 kN/m341 pliDie C
Compression Set 17 %
@Temperature 100 °C,
Time 79200 sec
17 %
@Temperature 212 °F,
Time 22.0 hour
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Temperature 160 °C
0.250 hour
@Temperature 320 °F
 
Descriptive Properties
Formulation as Tested0.5Stearic Acid
 100Millathane 76
 20N-220 Black
 4Di-Cup 40C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.25 PHR Zinc Stearate
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with TP-95
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Sulfur
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber
Lanxess Urepan® 643 G Polyurethane Rubber

PMILL044 / 87088

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.