Product Description: 60% long strand glass fiber reinforced nylon 6 Natural Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Filler/Reinforcement: Glass Fiber Uses: Automotive Applications Forms: Pellets Processing Method: Injection Molding Information provided by Celanese |