MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Invista P6G2Z-103 PP Impact Copolymer, Blow Molding, Extrusion, and Thermoforming
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Blow Molding Grade; Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Excellent impact. Produced without animal derived components.

Applications: Extruded sheet, profile extrusion, hot fill and retort applications, household chemicals and industrial parts

Regulatory: FDA – 21 CFR 177.1520(c) 3.1a

Information provided by INVISTA.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 1.80 g/10 min1.80 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 79.079.0ASTM D785
Tensile Strength, Yield 27.0 MPa3920 psiASTM D638
Elongation at Yield 8.80 %8.80 %ASTM D638
Flexural Modulus 1.158 GPa168.0 ksiSecant; ASTM D790
 1.225 GPa177.7 ksiTangent; ASTM D790
Izod Impact, Notched NBNBASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 - 165 °C320 - 329 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C190 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 200 °C392 °FTransition, Extrusion
 205 °C401 °FMetering, Extrusion
Rear Barrel Temperature 188 °C370 °FExtrusion
Head Temperature 210 °C410 °FExtrusion
Mold Temperature 16.0 °C60.8 °FExtrusion
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Air Pressure10 psiPre-Blow, Extrusion
 90 psiBlow Air, Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PINVIST975 / 325423

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.