MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grivory® XE 4065 black 9238 PA*-GF50
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product description: Grivory XE 4065 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewable raw materials. ISO polymer designation: PA 10T/X ASTM designation: PPA, polyphthalamide. The main distinguishing features of Grivory HT, when compared to other polyamides, are its good performance at high temperatures. Parts made of Grivory HT provide high stiffness and heat distortion temperatures. Further attributes of Grivory HT are the low moisture absorption, good dimensional stability and excellent chemical resistance.G rivory XE 4065 is especially suitable for parts in the following application areas:
  • Electro / Electronics
  • Automotive
  • Industrial
  • Safety equipment
  • Household

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.58 g/ccDry; ISO 1183
Water Absorption 1.7 %Sim. to ISO 62
Moisture Absorption 0.800 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 245 MPaDry; ISO 2039-1
 245 MPaConditioned; ISO 2039-1
Tensile Strength at Break 220 MPaConditioned; ISO 527-1/-2
 230 MPaDry; ISO 527-1/-2
Elongation at Break 2.5 %Dry; ISO 527-1/-2
 2.5 %Conditioned; ISO 527-1/-2
Tensile Modulus 16000 MPaDry; ISO 527-1/-2
 16000 MPaConditioned; ISO 527-1/-2
Charpy Impact Unnotched 80.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
 80.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 90.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
 90.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
Charpy Impact, Notched 12.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 12.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 12.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmDry; IEC 60093
 1.00e+10 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 31.0 kV/mmConditioned; IEC 60243-1
 32.0 kV/mmDry; IEC 60243-1
Comparative Tracking Index 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°CISO 11359-1/-2
Melting Point 295 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 150 °CLong Term; ISO 2578
 250 °CShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 270 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 225 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 HB
@Temperature 1.50 °C
IEC 60695-11-10
 
Descriptive Properties
AutomotiveAir intake systems
 Compressed air systems
 Cooling and climate control
 Fuel systems
 Hydraulic systems
 Interior
 Powertrain and Chassis
Electricals & ElectronicsElectrical equipment
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
 Mechanical Engineering
 Power transmission
 Tools & Accessories
ProcessingInjection Molding
Product AttributesBio based Polyamide
 Hydrolysis resistant
 Improved alcohol resistance
 Partially aromatic Polyamide
Special CharacteristicsImproved heat resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Crastin® LW9030 BK851 PBT+ASA-GF30
EMS-Grivory Grivory® HTV-5H1 black 9205 PA6T/6I-GF50
EMS-Grivory Grivory® HTV-3H1 black 9205 PA6T/6I-GF30
DuPont Mobility and Materials Zytel® HTN 52G45HSL NC010 Polyphthalamide (PPA)
EMS-Grivory Grivory® XE 4063 black 9238 PA6T/66-GF30

PGRH404 / 157113

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.