MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Zortrax Z-NYLON Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Z-NYLON is a versatile and strong 3D printing filament resistant to high temperatures and various chemicals. It can be post-processed with tools meant for machining metals. Z-NYLON is hard to break and easy to paint as it can be colored with commonly used, acid-based clothing dyes. The filament quickly absorbs moisture and should be stored in a water-proof bag with a moisture absorber. As all nylon-based materials, Z-NYLON has a relatively high shrinkage so it is not advisable to use it for 3D printing large geometric shapes with steep slopes. To reduce the shrinkage, it is recommended to work with HEPA Cover attached on the M Series Plus 3D printers.

Information provided by Zortrax

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.027 g/cc0.03710 lb/in³ISO 1183-3:2003
Melt Flow 9.23 g/10 min
@Load 5.00 kg,
Temperature 235 °C
9.23 g/10 min
@Load 11.0 lb,
Temperature 455 °F
ISO 1133:2006
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6262ISO 868:1998
Tensile Strength at Break 29.71 MPa4309 psiISO 527:1998
Tensile Strength 33.22 MPa4818 psiISO 527:1998
Elongation at Break 23.62 %23.62 %ISO 527:1998
Elongation at Yield 9.17 %9.17 %ISO 527:1998
Flexural Strength 38.3 MPa5550 psiISO 178:2011
Flexural Modulus 0.78101 GPa113.28 ksiISO 178:2011
Izod Impact, Notched (ISO) 12.81 kJ/m²6.096 ft-lb/in²ISO 180:2004
 
Thermal PropertiesMetricEnglishComments
Melting Point 172.81 °C343.06 °FISO 11357-3:2014

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZORT003 / 281882

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.