MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Durethan® B 31 F 000000 Nylon 6, Film Grade
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Film Grade

Material Notes: PA 6, film grade, low viscosity, easy flow, additive-free

Application Examples: flat and blown film, monofilaments, coatings

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183
Water Absorption 10 %Test Sim. to ISO 62
Moisture Absorption at Equilibrium 3.0 %23°C/50% R.H.; Test Sim. to ISO 62
Viscosity Number 155 cm³/gISO 307, 1157, 1628
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 235 °C
Estimated using room temperature density; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 35.0 MPaConditioned; ISO 527-1/-2
 75.0 MPaISO 527-1/-2
Elongation at Break 20 %Nominal; ISO 527-1/-2
 >= 50 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 4.0 %ISO 527-1/-2
 25 %Conditioned; ISO 527-1/-2
Tensile Modulus 800 MPaConditioned; ISO 527-1/-2
 2800 MPaISO 527-1/-2
Charpy Impact Unnotched 55.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 5.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 <= 5.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 5.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 50.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmConditioned; IEC 60093
 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.5
@Frequency 1e+6 Hz
IEC 60250
 3.9
@Frequency 100 Hz
IEC 60250
 4.0
@Frequency 1e+6 Hz
Conditioned; IEC 60250
 18
@Frequency 100 Hz
Conditioned; IEC 60250
Dielectric Strength 30.0 kV/mmIEC 60243-1
 35.0 kV/mmConditioned; IEC 60243-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 80.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°CISO 11359-1/-2
Melting Point 222 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 150 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 40.0 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 HB
@Thickness 3.20 mm
IEC 60695-11-10
Oxygen Index 24 %ISO 4589-1/-2
 
Descriptive Properties
FormPellets
ISO Short NameISO 1874: PA 6,FN,14,030
ProcessingFilm extrusion
RegionAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Vestamid® L1901 nf (dry properties) Nylon 12
DuPont Teijin Films Mylar® MO21 Polyester Film, 900 Gauge
DuPont Teijin Films Mylar® MO21 Polyester Film, 1000 Gauge

PLANX0722 / 98937

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.