Isocor™ SVP4007 is a high viscosity PA-6. This resin is specifically suited for applications requiring excellent abrasion, tensile and elongation properties. This resin can be processed using conventional techniques. Used for profile extrusions, film extrusions, flexible tubing, fiber and filaments. Information provided by Shakespeare Company. |