MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Kraiburg TPE THERMOLAST® K TF9AAC Natural TPE  (Unverified Data**)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes:
  • Natural compound with BgVV/FDA compliance
  • Excellent mechanical properties
  • Easy to color

Typical Applications:

  • Esthetic and functional packaging elements
  • Cosmetics and wellness products
  • Parts with food contact (e.g. seals, wine corks)
  • Medical parts

Material Advantages:

  • BgVV/FDA compliant
  • Easy to color
  • Good adhesion to PP and engineering thermoplastics
  • PVC free
  • Low density
  • Good Elasticity
  • Excellent flow behavior

Processing:

  • Like polyolefins
  • No predrying

Information provided by Kraiburg TPE.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³DIN 53479
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8686DIN 53505
Tensile Strength at Break 12.0 MPa1740 psiDIN 53504
Elongation at Break 600 %600 %DIN 53504
Tear Strength 32.0 kN/m183 pliDIN 53515
Compression Set  60 %
@Temperature 70.0 °C
60 %
@Temperature 158 °F
24 hours; ISO 815
 80 %
@Temperature 100 °C
80 %
@Temperature 212 °F
24 hours; ISO 815
 40 %
@Temperature 23.0 °C,
Time 259000 sec
40 %
@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 220 °C356 - 428 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
ColorNatural

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKRAIB072 / 49219

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.