MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eastman Tritan™ MXF121-17054X White Medical Grade Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Tritan™ MXF121 copolyester is an amorphous opaque product. Tritan MXF121 contains a mold release derived from vegetable based sources. Tritan MXF121 has many outstanding features that include excellent toughness, hydrolytic stability, heat resistance, chemical resistance, and melt flowability. Tritan MXF121 has been formulated for medical devices. Tritan MXF121 has passed FDA/ISO 10993 testing for cytotoxicity, skin sensitization, and intracutaneous reactivity.

Applications

  • Medical equipment
  • Medical housings and hardware
Key Attributes
  • Ease of processing
  • Excellent hydrolytic stability
  • Fast cycle times
  • Fast drying times
  • Good chemical resistance
  • Good heat resistance
  • Good melt flowability
  • Good toughness

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D792
Linear Mold Shrinkage 0.00300 - 0.00600 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 109ASTM D785
Tensile Strength at Break 47.0 MPaASTM D638
Tensile Strength, Yield 43.0 MPaASTM D638
Elongation at Break 133 %ASTM D638
Elongation at Yield 6.00 %ASTM D638
Tensile Modulus 1605 MPaASTM D638
Flexural Modulus 1748 MPaASTM D790
Izod Impact, Notched 183 J/mASTM D256
Izod Impact, Unnotched NBASTM D4812
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °CASTM D648
Flammability, UL94 V-2
@Thickness 1.50 mm
 V-2
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 275 °C
Mold Temperature 24.0 - 66.0 °C
Drying Temperature 88.0 °C
Dry Time 4.00 - 6.00 hour
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM4188 / 323811

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.