MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dover Chemical DOVERPHOS 9 Diphenyl Isooctyl Phosphite
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Doverphos 9 is diphenyl isooctyl phosphite (DPIOP). Doverphos 9 has the lowest molecular weight, and therefore the highest phosphorus content of our commercially available alkyl-aryl phosphites. Doverphos 9 is an effective liquid phosphite heat stabilizer for polyurethanes, coatings, ABS, and polycarbonates. Typical use levels range from 0.1 to 3.0% for most applications. Doverphos 9 can be used in rigid and flexible PVC applications as a secondary stabilizer to give brighter, more consistent colors and improve heat stability of PVC. Use levels in PVC range from 0.25 to 1.00%.

Information provided by DoverChem

Key Words: CAS# 26401-27-4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 - 1.047 g/cc
@Temperature 25.0 °C
1.04 - 1.047 g/cc
@Temperature 77.0 °F
Molecular Weight 346 g/mol346 g/mol
ASTM Color <= 50<= 50APHA
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.050<= 0.050[mgKOH/gm]
 
Optical PropertiesMetricEnglishComments
Refractive Index <= 1.524
@Temperature 25.0 °C
<= 1.524
@Temperature 77.0 °F
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 9.0 %9.0 %
 
Descriptive Properties
Physical FormClear liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WDOVER035 / 217654

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.