MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Chesterton 651 Detergent Lubricating Oil
Categories: Fluid; Lubricant

Material Notes: Description: Chesterton® 651 Detergent Lubricating Oil is the plant-wide product of choice for superior-quality, low-viscosity, industrial lubricating needs. It is a cost-effective oil with high detergency that cleans as it protects and prolongs the life of all types of equipment. The superactive formula results in maximum penetration and surface wetting into the tightest friction spots, providing long-lasting protection against wear. It quickly penetrates tight tolerances and removes old varnish deposits and buildup caused by conventional lubricants. 651 Detergents Lubricating Oil is so effective at getting rid of old lubricant residues that it is routinely used as a cleaning aid to wipe down parts and equipment and leave a protective, oily film. This multi-purpose lubrication is used in any industry where the potential for friction and wear exists. It is ideal for thin film lubrication of moving equipment, machinery, electric motors, sensitive instruments, assembly lines, door hinges and other devices that require a lubricant with high detergency.

Features:

  • Cleans as it lubricates
  • Will not build up
  • Penetrates close tolerances
  • Will not gum up delicate parts
  • Ideal for high-speed industrial bearings
  • Special additives for longer life
  • NSF H2 - Registration number 133946 (bulk) and 133928 (aerosol)

Benefits:

  • Save production time
  • Reduce maintenance costs
  • Save the cost of replacement parts
  • Prolong the life of machinery and parts
  • Significantly reduce power consumption
  • Safe to use; easy to use

Applications: 651 Detergent Lubricating Oil is a high-quality, light-grade, multipurpose lubricant for all types of plant equipment, electric motors and machinery as well as sensitive instruments like chronometers, amplifiers and tape recorders. It can be used plant-wide in machine shops, maintenance shops, instrument repair shops, boiler rooms and assembly lines, wherever a high-detergency lubricant is desired. It works exceptionally well in oil-lubricated pneumatic systems. The primary reason for failure in these systems are sticking pistons and worn seals. When 651 Detergent Lubrication Oil is used as a direct replacement for the standard hydraulic oil, reductions of up to 90% in typical pneumatic maintenance costs can be achieved. The increase in systems uptime and reduction in rejected parts mean additional cost savings.

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/cc
Kinematic Viscosity at 40°C (104°F) 22 cSt22 cStASTM D445, DIN 51 561
 
Mechanical PropertiesMetricEnglishComments
Four Ball Wear 0.430 mm
@Temperature 75.0 °C,
Time 3600 sec
0.0169 in
@Temperature 167 °F,
Time 1.00 hour
1200 rpm, 40 kg, scar diameter; ASTM D2266, DIN 51 350
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -23.0 °C-9.40 °F
Pour Point -29.0 °C-20.2 °FASTM D97, ISO 3016
Flash Point 127 °C261 °FASTM D93, DIN 51 755
 
Descriptive Properties
AppearanceAmber Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTCHS079 / 138191

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.