MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

TOSAF Compounds Tosaf EH9201S Polyolefin, Masterbatch
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: EH9201S MB is suitable for coloring of extruded film, molded and blowing made of Various Types of Polyolefin. Economical grade with high color strength equivalent to 40% SRF

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

RoSH Compliance: RoSH Compliant

Additives Category: Masterbatch – Pigment – Black

Carrier Resin: Polyethylene or ethylene-olefin copolymer (PE)

Recommended for Use In: Polyethylene or ethylene-olefin copolymer (PE); Polypropylene or propylene-olefin copolymer (PP)

Form: Pellets/Granules

Chemical Description: Carbon Black

State at Room Temperature: Solid

Information provided by TOSAF Compounds Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.799 - 0.900 g/cc0.0289 - 0.0325 lb/in³
Density 1.20 - 1.30 g/cc0.0434 - 0.0470 lb/in³ASTM D792
Melt Flow 1.0 - 7.0 g/10 min
@Load 10.0 kg,
Temperature 190 °C
1.0 - 7.0 g/10 min
@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Melting Point 140 - 150 °C284 - 302 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 300 °C<= 572 °F
 
Descriptive Properties
Additive Concentration71-23%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTOSAF1499 / 312192

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.