Hifax TRC 134P C6 C12594 is a 20% talc filled PP copolymer, with very low shrinkage, good impact resistance and high UV resistance. Product is available as a customized color matched, pellet form. This grade is delivered in C12594 color version. Availability: Asia-Pacific Application: Bumpers Market: Automotive Processing Method: Injection Molding Attribute: Good Impact Resistance; Good UV Resistance; Low Coefficient of Linear Thermal Expansion; Low Shrinkage Information provided by LyondellBasell. |