MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Copper nickel 20%, UNS C71000, OS025 Temper, Flat Products & Tubing
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Nominal Grain Size 0.025 mm

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Gas Shielded Arc Welding, Spot Weld, Seam Weld, Butt Weld; Good Suitability – Coated Metal Arc Welding, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Fair Suitability – Oxyacetylene Welding

Common Fabrication Processes: Blanking; Forming and Bending; Welding

Typical uses: Communication Relays; Resistance Wire; Resistors; Springs; Condenser Plates; Condensers; Evaporator Tubing; Evaporators; Ferrules; Heat Exchanger Tubes

Applicable Specifications: Bar – SAE J461, SAE J463, ASTM B122/B122M; Bolts – ASTM F468; Heat Exchanger Tube – ASME SB543; Nuts - ASTM F467; Pipe – ASME SB466, ASTM B466/B466M; Plate – ASTM B122/B122M; Screws – ASTM F468; Sheet – ASTM B122/B122M, SAE J461, SAE J463, ASTM B694; Strip – ASTM B122/B122M, SAE J461, SAE J463, ASTM B694; Studs – ASTM F468; Tube - Condenser Tube SAE J463, ASME SB359, ASME SB395, ASTM B359/B359M, Condenser Tube ASTM B111/B111M, Condenser Tube SAE J461, ASTM B395/B395M, ASME SB466, ASTM B543/B543M, ASTM B466/B466M, Condenser Tube ASME SB111; Welded Heat Exchanger & Condenser Tube – ASTM B956/B956M; Wire - ASTM B206/B206M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.323 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 49.0 ksi
 53.0 ksi
@Thickness 1.02 mm
Tensile Strength, Yield 18.0 ksi0.5% Ext
 16.0 ksi
@Thickness 1.02 mm
0.2% Offset
Elongation at Break 40 %
 35 %
@Thickness 1.02 mm
Tensile Modulus 20000 ksi
Modulus of Rigidity 7500 ksi
Poissons Ratio 0.33Calculated
Machinability 20 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000260 ohm-cm6.5% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.10 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 21.0 BTU-in/hr-ft²-°F
Melting Point 2100 - 2190 °F
Solidus 2100 °F
Liquidus 2190 °F
Annealing Point 1200 - 1500 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 74 - 81 %As Balance
Iron, Fe <= 1.0 %
Lead, Pb <= 0.050 %
Manganese, Mn <= 1.0 %
Nickel, Ni 19 - 23 %
Zinc, Zn <= 1.0 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC71000x1 / 293092

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.