MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Dioshy TPO F955D-OS Thermoplastic olefin
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Thermoplastic olefin (TPO), very popular in Japanese markets, hardness range Shore A 85 ~ Shore D 63.

Features:

  • Possessed excellent heat resistance and elastic property, good chemical resistance, weather resistance and aging resistance.
  • Mostly applied for car parts.
  • Good anti-slip property, especially in wet status; very good compression set; white color and good coloring property.
  • Passed US FDA and EU LFGB food application standards, medical grades are also included.
  • Very good resilience ability and good tensile strength; semi-transparency, good coloring property; customized.
  • Suitable to dual color processing for PP or PE; also can be the toughener for PP or PE.
  • Suitable to mostly thermoplastic procedures; PVC replacement.
  • Green material, passed heavy metal regulation, RoHS and EACH –SVHC

      Information provided by DIOSHY CO., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.891 g/cc0.891 g/ccJIS-K6301
Melt Flow 6.72 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.72 g/10 min
@Load 4.76 lb,
Temperature 374 °F
JIS-K7210
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555JIS-K6301
Tensile Strength 13.3 MPa1930 psiJIS-K6310
Elongation at Break 784 %784 %JIS-K6310
100% Modulus 10.8 MPa1560 psiJIS-K6310
300% Modulus 3.63 MPa526 psiJIS-K6310
Tear Strength 1331 kN/m7601 pliJIS-K6310-B
Compression Set 32 %
@Temperature 23.0 °C,
Time 79200 sec
32 %
@Temperature 73.4 °F,
Time 22.0 hour
JIS-K6301
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 165 - 180 °C329 - 356 °FInjection
 170 - 180 °C338 - 356 °FExtrusion
Middle Barrel Temperature 185 - 195 °C365 - 383 °FInjection
 185 - 195 °C365 - 383 °FExtrusion
Front Barrel Temperature 185 - 195 °C365 - 383 °FInjection
 185 - 195 °C365 - 383 °FExtrusion
Nozzle Temperature 195 - 215 °C383 - 419 °FInjection
Die Temperature 195 - 215 °C383 - 419 °FExtrusion
Drying Temperature 90.0 °C194 °F
Dry Time 1.00 hour1.00 hour
 
Descriptive Properties
Application Dual color processingPE
ColorTranslucent
TPS typeTPO-I

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDIOSH057 / 294667

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.