MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Empilon EMPILON® HNT250 TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: EMPILON®HAR series is mainly used to bond with engineering plastics, such as ABS, PC, Nylon, PETG, PBT, etc., it has excellent tactile feelings, matte surface texture, shock absorption and anti-slip. Usually widely be utilized in electronics or hand tool industry. It is a blending material based on modified hydrogenated Styrenic block copolymer, with a hardness range from Shore A39 to Shore A85. Its main processing method is double injection or co-extrusion. The series is non-toxic. It does not contain RCRA 8 heavy metals, halogens, phthalate and is 100% recyclable and eco-friendly. It can pass the European Union Waste Electronics and Electrical Equipment (WEEE), Restriction of Hazardous Substances (RoHS) regulations and meet the environmental requirements of SONY SS-00259 4th Edition. This series owns excellent mechanical property, weather and heat resistance, good resilience and has low specific gravity, good chemical resistant and hydrolysis resistant performance. HAR series products need to be dried with hot air at 80-90? (dehumidification and drying is recommended) for at least 2 hours before processing, and drying is required during injection molding process. When you want to dye this series of products, please choose PE or EVA as the substrate of masterbatch, and never use PVC as the base material. In addition, please use a higher screw speed and higher back pressure to achieve better dispersion of the colorant.

Series Features:

  • Excellent Heat Aging Resistance
  • Low Specific Gravity
  • Excellent Mechanical Properties and Toughness
  • High Transparency
  • Excellent Resilience
  • Extremely Low Hardness
  • Apply to high toughness, high elastic recover demand product
  • Apply to high transparent elastic product
  • Apply to medical food grade products
  • Injection molding, extrusion molding, calendaring and other processing technology
Applications:
  • Mobile Phone Case: Comfortable tactile feeling
  • Electronics handle: Aesthetic/Comfortable tactile feeling
  • Hand Tools Handle: Comfortable tactile feeling
  • Electrical Tools Handle: Comfortable tactile feeling
  • Swim/Ski Goggles: Comfortable tactile feeling/Good sealing performance
  • Sporting Camera Shell: Outstanding quality/Comfortable tactile feeling

Information provided by EMILON®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Melt Flow >= 3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
>= 3.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 49
@Time 10.0 sec
49
@Time 0.00278 hour
ASTM D2240
Tensile Strength 2.94 MPa427 psiASTM D412
Elongation at Break 500 %500 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -50.0 °C-58.0 °F
Shrinkage, MD 1.9 %1.9 %
Shrinkage, TD 2.3 %2.3 %
 
Processing PropertiesMetricEnglishComments
Feed Temperature 240 - 255 °C464 - 491 °F
Middle Barrel Temperature 250 - 265 °C482 - 509 °F
Front Barrel Temperature 255 - 265 °C491 - 509 °F
Nozzle Temperature 260 - 270 °C500 - 518 °F
Melt Temperature 240 - 270 °C464 - 518 °F
 <= 290 °C<= 554 °Fdo not exceed
Mold Temperature 25.0 - 40.0 °C77.0 - 104 °F
Injection Pressure 4.41 - 5.88 MPa640 - 853 psi
Back Pressure 0.490 - 0.981 MPa71.1 - 142 psi
 
Descriptive Properties
AdhesionPA66
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEMPIL042 / 294729

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.