MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Multiflex™ TES ABPLAST MT230765 Styrenic Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Thermoplastic Elastomer based Styrenic

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.880 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.013 cm/cmISO 294-4, 2577
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 34
@Time 15.0 sec
ISO 7619-1
Tensile Strength at Break 13.0 MPaISO 527-1/-2
Elongation at Break 180 %ISO 527-1/-2
Flexural Modulus 230 MPaISO 178
Tear Strength 75.0 kN/mparallel; ISO 34-1
 45.0 kN/m
@Temperature 80.0 °C
ISO 34-1
 150 kN/m
@Temperature -30.0 °C
ISO 34-1
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 °COptimum, Injection
Mold Temperature 20.0 - 50.0 °CInjection
 35.0 °COptimum, Injection
Drying Temperature 65.0 °C
@Time 7200 - 14400 sec
Injection; Dehumidified Dryer
Back Pressure 1.00 MPa
Shelf Life 12.0 Month
 
Descriptive Properties
CompatibilityPolyolefins
Delivery formPellets
Drying Recommendedyes
FeaturesPaintable
Flow length (mm)275
Hold pressure rangeas low as possibleInjection
 as low as possibleInjection
Injection speedMedium-High
ProcessingInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDTF9316 / 254365

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.