MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Dow Nucrel™ AN4211-5C Ethylene Methyl Acrylate Acrylic Acid
Categories: Polymer; Thermoplastic

Material Notes: Product Description: Nucrel™ AN4211-5C resins are acid modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet from for use in conventional extrusion equipment designed to process polyethylene (PE) resins.
Features:
  • Better adhesion to aluminum metalized films, such as VM-CPP, without delamination between metalized aluminum and CPP
  • Excellent processability at lower temperature, such as 200-220°C
Characteristics/Benefits: It is designed to have good adhesion to metalized CPP in extrusion coating operation without delamination between metalized aluminum and CPP. Typical adhesions to VM-CPP are shown below. Customer should conduct their own adhesion comparison to ensure these materials meet their performance.

Applications:

  • Nucrel™ AN4211-5C series resins adhere to a wide variety of materials. They are most often used to adhere to PE, EVA, Polyamide, ionomer, paper, aluminum foil, and printed films.
  • It is designed for low melt temperature extrusion coating/laminating applications
  • Common usage in snack applications, as a OPP/VM-CPP tie layer.

    Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

    Agency Ratings: FDA 21 CFR 177.1330 (a)

    Form: Pellets

    Processing Method: Coextrusion; Extrusion Coating; Laminating

    Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccISO 1183
 0.932 g/ccASTM D792
Melt Flow 32 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 32 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 201 °FPeak; ASTM D3418
 201 °FISO 3146
Vicat Softening Point 153 °FASTM D1525
 153 °FISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF555 / 311248

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.