MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Special Metals INCOLOY® Alloy 903
Categories: Metal; Superalloy; Iron Base

Material Notes: A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion at temperatures to about 800°F (430°C). It also has a constant modulus of elasticity and is highly resistant to thermal fatigue and thermal shock. Used in gas turbines for rings and casings. Standard product forms are round, flats, forging stock, sheet, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: UNS N19903; AFNOR Z3 NK 38
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.25 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1310 MPaPrecipitation Hardened
Tensile Strength, Yield 1100 MPa
@Strain 0.2 %
Precipitation Hardened
Elongation at Break 14 %Precipitation Hardened
Modulus of Elasticity 146.8 GPa
@Temperature 0.000 °C
 146.9 GPa
@Temperature -50.0 °C
 146.9 GPa
@Temperature 50.0 °C
 147.2 GPa
@Temperature 100 °C
 147.4 GPa
@Temperature -100 °C
 147.8 GPa
@Temperature 150 °C
 148.4 GPa
@Temperature 200 °C
 148.9 GPa
@Temperature -195 °C
 149.3 GPa
@Temperature 250 °C
 149.8 GPa
@Temperature 600 °C
 150.2 GPa
@Temperature 300 °C
 151.3 GPa
@Temperature 350 °C
 151.8 GPa
@Temperature 550 °C
 152.4 GPa
@Temperature 400 °C
 153.5 GPa
@Temperature 450 °C
 153.9 GPa
@Temperature 500 °C
Poissons Ratio 0.226
@Temperature 250 °C
 0.227
@Temperature 300 °C
 0.231
@Temperature 200 °C
 0.236
@Temperature 350 °C
 0.239
@Temperature 50.0 °C
 0.241
@Temperature 400 °C
 0.242
@Temperature 150 °C
 0.247
@Temperature 100 °C
 0.273
@Temperature 450 °C
 0.30
@Temperature 500 °C
 0.318
@Temperature 550 °C
 0.352
@Temperature 600 °C
Shear Modulus 55.4 GPa
@Temperature 600 °C
 57.6 GPa
@Temperature 550 °C
 59.0 GPa
@Temperature 100 °C
 59.2 GPa
@Temperature 500 °C
 59.3 GPa
@Temperature 50.0 °C
 59.5 GPa
@Temperature 150 °C
 60.3 GPa
@Temperature 200 °C
 60.3 GPa
@Temperature 450 °C
 60.9 GPa
@Temperature 250 °C
 61.2 GPa
@Temperature 300 °C
 61.2 GPa
@Temperature 350 °C
 61.4 GPa
@Temperature 400 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000610 ohm-cm
 0.0000650 ohm-cm
@Temperature 50.0 °C
 0.0000735 ohm-cm
@Temperature 100 °C
 0.0000880 ohm-cm
@Temperature 200 °C
 0.000102 ohm-cm
@Temperature 300 °C
 0.0001135 ohm-cm
@Temperature 400 °C
 0.0001195 ohm-cm
@Temperature 500 °C
 0.000122 ohm-cm
@Temperature 600 °C
Curie Temperature 415 - 470 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.65 µm/m-°C
@Temperature 25.0 - 427 °C
Specific Heat Capacity 0.435 J/g-°Ctest temperature not reported
 0.442 J/g-°C
@Temperature 50.0 °C
 0.454 J/g-°C
@Temperature 100 °C
 0.482 J/g-°C
@Temperature 200 °C
 0.507 J/g-°C
@Temperature 300 °C
 0.532 J/g-°C
@Temperature 400 °C
 0.559 J/g-°C
@Temperature 500 °C
 0.584 J/g-°C
@Temperature 600 °C
Thermal Conductivity 16.7 W/m-Ktest temperature unknown
 16.9 W/m-K
@Temperature 50.0 °C
 17.2 W/m-K
@Temperature 100 °C
 17.9 W/m-K
@Temperature 200 °C
 18.3 W/m-K
@Temperature 300 °C
 19.0 W/m-K
@Temperature 400 °C
 20.3 W/m-K
@Temperature 500 °C
 21.9 W/m-K
@Temperature 600 °C
Melting Point 1318 - 1393 °C
Solidus 1318 °C
Liquidus 1393 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.90 %
Cobalt, Co 15 %
Iron, Fe 42 %
Nickel, Ni 38 %
Niobium, Nb (Columbium, Cb) 3.0 %
Titanium, Ti 1.4 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals INCOLOY® Alloy 909
Special Metals INCOLOY® Alloy 907
RSP Technology RSA-473 AH Aluminum Super Alloy
Special Metals NI-SPAN-C® Alloy 902
Haynes Waspaloy™ alloy, sheet

NINC84 / 17427

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.