Product Description: LD 331.08 is a 5.9% vinyl acetate copolymer, higher clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability. Availability: Latin America, North America and South America Additive: - Antiblock: No
- Slip: No
- Thermal Stabilizer: Yes
Applications: - Coextrusion Films
- Foams
- Form Fill and Seal Packaging
- Freezer Film
- High Clarity Film
- Lamination Film
- Poultry Bag
- Produce Bags
- Rice Bags
Information provided by ExxonMobil |