MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Copper Alloy, UNS C42230, BW33520, H04 Temper, Strip
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Hard

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Gas Shielded Arc Welding, Butt Weld, Capacity for Being Hot Formed; Fair Suitability – Oxyacetylene Welding

Typical Uses: Conductors; Terminals Connectors

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.75 g/cc0.316 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 197
@Load 3.00 kg
197
@Load 6.62 lb
Tensile Strength 580 - 636 MPa84100 - 92300 psi
 646 MPa93700 psiTypical
Tensile Strength, Yield 567 MPa82200 psi0.2% Offset, Typical
 550 - 640 MPa79800 - 92800 psi0.2% Offset
Tensile Modulus 119 GPa17300 ksi
Modulus of Rigidity 44.34 GPa6431 ksiCalculated
Poissons Ratio 0.3450.345
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000510 ohm-cm0.00000510 ohm-cm34% IACS
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 10.5 W/m-K73.2 BTU-in/hr-ft²-°F
Melting Point 1004 - 1060 °C1839 - 1940 °F
Solidus 1004 °C1839 °F
Liquidus 1060 °C1940 °F
 
Component Elements PropertiesMetricEnglishComments
Cobalt, Co 0.30 - 1.5 %0.30 - 1.5 %
Copper, Cu 87 - 91 %87 - 91 %
Iron, Fe <= 0.050 %<= 0.050 %
Lead, Pb <= 0.010 %<= 0.010 %
Manganese, Mn <= 0.050 %<= 0.050 %
Silicon, Si 0.050 - 0.30 %0.050 - 0.30 %
Tin, Sn 0.40 - 1.5 %0.40 - 1.5 %
Zinc, Zn 5.6 - 12.3 %5.6 - 12.3 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC42230x1 / 291930

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.