MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Phillips 66 ISO Grade 220 Food Machinery Oil
Categories: Fluid; Lubricant

Material Notes: Food Machinery Oil is a premium quality, ashless, food-grade lubricant specially developed for use in hydraulic systems, rotary air compressors, lightly to moderately loaded enclosed gear drives and other machinery in food processing and beverage plants. All viscosity grades are registered by NSF International as H1 lubricants for use where incidental food contact may occur, and also as H2 lubricants for use in applications where there is no chance for incidental food contact. All viscosity grades are certified as meeting Canadian Food Inspection Agency requirements for use in federally registered food plants, and also are certified Kosher and Pareve. Food Machinery Oil is manufactured with hydroprocessed base oils of the highest purity and fortified with an ashless (zinc-free) antiwear additive plus rust and oxidation inhibitors. It provides excellent wear protection, corrosion resistance and deposit control to ensure long service life for hydraulic pumps and motors and other equipment. It has good water-separating properties to minimize the formation of emulsions, and is resistant to excessive foaming. Food Machinery Oil meets the performance requirements of all major hydraulic pump manufacturers, and is recommended for use in all types of high-pressure, high-speed hydraulic pumps.

Applications:

  • Food processing equipment in bakeries, canneries, meat packing plants and bottling plants
  • Hydraulic systems, circulating oil systems and rotary air compressors (typically, ISO VG 68 and lighter)
  • Lightly to moderately loaded enclosed industrial gear drives that do not require a compounded or extreme-pressure (EP) gear oil (typically, ISO VG 100 and heavier)
  • Air tools and other pneumatic equipment lubricated through air line lubricators
  • Chain drives
  • Deep well water pumps
  • Equipment on offshore oil platforms
Food Machinery Oil meets the requirements of the following government and industry specifications:
  • Canadian Food Inspection Agency (CFIA) requirements for use in federally registered food plants (incidental food contact) (registered)
  • FDA 21 CFR 178.3570 for incidental food contact
  • NSF International H1 and former 1998 USDA H1 guidelines for incidental foodcontact (Registration Nos. 137567, 137568, 137569, 140092, 140093)
  • NSF International H2 and former 1998 USDA H2 guidelines for use with no chance of incidental food contact
Features/Benefits:
  • Excellent wear protection for critical system components
  • Good oxidation resistance to minimize sludge and varnish formation
  • Protects against rust and corrosion
  • Good water-separating properties to minimize the formation of emulsions
  • Good foam resistance
  • Certified Kosher and Pareve

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.876 g/cc0.876 g/cc
Density 0.874 g/cc0.0316 lb/in³
Viscosity Measurement 121121Index
Saybolt Viscosity at 100°F 1151 SUS1151 SUS
Saybolt Viscosity at 210°F 110 SUS110 SUS
Kinematic Viscosity at 40°C (104°F) 220 cSt220 cSt
Kinematic Viscosity at 100°C (212°F) 22 cSt22 cSt
Oxidative Stability 50 hour50 hourTOST; ASTM D943-04a
 480 hour480 hourRPVOT; ASTM D2272
ASTM Color 0.500.50L; ASTM D1500
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.0500.050[mg KOH/g]; ASTM D974
 
Mechanical PropertiesMetricEnglishComments
Four Ball Wear 0.500 mm0.0197 inScar Diameter; ASTM D4172
 
Thermal PropertiesMetricEnglishComments
Pour Point -9.00 °C15.8 °F
Flash Point 263 °C505 °FCOC
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
USDA YesYes
 
Descriptive Properties
Color+30Saybolt
Copper Corrosion1aASTM D130
Demulsibility30 minutes to passASTM D1401
FZG Scuffing Test12 Failure Load StageASTM D5182

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON6087 / 210126

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.