MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Skychem S7021 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Features: Tpu (thermoplastic polyurethane elastomer) is a kind of heating can be plasticizing, solvent dissolved elastomer, excellent abrasion resistance, excellent ozone resistance, high hardness, high strength, good elasticity, good low temperature resistance, good resistance to oil, chemicals, in the humid environment type polyether ester hydrolysis stability compared with polyester is better, more environmental protection and other excellent comprehensive performance.

Areas of application: Because of its good processing performance, widely used in national defense, medical, food and other industries, with the development of economy and consumption upgrade, will gradually replace traditional materials, consumption is increasing year by year. Especially TPU film as a segment of the market of polyurethane products, use is becoming more and more widely in recent years, in cars, clothing, shoes, outdoor sports, medical, electronics, bulletproof glass, oil transportation, industrial and other industries have a wide range of applications.. With thermoplastics can be used the same technology and equipment to processing, such as injection molding, extrusion, blow molding, calendar in etc., especially suitable for mass production of medium and small size parts. Waste materials can be recycled and reused, using different additives or fillers to improve certain physical properties and reduce costs.

Information provided by Shanghai Sukeyou chemical new raw materials Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7272ASTM D2240
Tensile Strength 20.0 MPa2900 psiASTM D412
Elongation at Break 750 %750 %ASTM D412
100% Modulus 2.80 MPa406 psiASTM D412
Tear Strength 93.0 kN/m531 pliASTM D412
Abrasion 100100[mm3]; DIN 53516

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSKYCHEM031 / 314387

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.