MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik Sanicro 28 fro OCTG Tube and pipe, seamless
Categories: Metal; Ferrous Metal; Alloy Steel; Austenitic

Material Notes: Sanicro 28 is a high-alloy austenitic stainless steel for OCTG down-hole applications in particularly corrosive conditions. The grade is characterized by:
  • Very good resistance to sulphide stress cracking and stress corrosion cracking (SCC) in chloride and sour (H S/Cl ) environments
  • Very high resistance to pitting and crevice corrosion

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C <= 33PSL2 Sanicro 28-110
 <= 35PSL2 Sanicro 28-125
 <= 35PSL1 Sanicro 28-110
 <= 37PSL1 Sanicro 28-125
Tensile Strength, Ultimate >= 795 MPaPSL1 Sanicro 28-110
 >= 798 MPaPSL2 Sanicro 28-110
 >= 895 MPaPSL2 Sanicro 28-125
 >= 895 MPaPSL1 Sanicro 28-125
Tensile Strength, Yield 760 - 965 MPa
@Strain 0.2 %
PSL1 Sanicro 28-110
 760 - 965 MPa
@Strain 0.2 %
PSL2 Sanicro 28-110
 860 - 1000 MPa
@Strain 0.2 %
PSL2 Sanicro 28-125
 860 - 1035 MPa
@Strain 0.2 %
PSL1 Sanicro 28-125
Elongation at Break >= 10 %PSL2 Sanicro 28-125
 >= 10 %PSL1 Sanicro 28-125
 >= 11 %PSL2 Sanicro 28-110
 >= 11 %PSL1 Sanicro 28-110
Modulus of Elasticity 174 GPa
@Temperature 300 °C
 182 GPa
@Temperature 200 °C
 190 GPa
@Temperature 100 °C
 195 GPa
@Temperature 20.0 °C
Poissons Ratio 0.29
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000950 ohm-cm
@Temperature 20.0 °C
 0.0000100 ohm-cm
@Temperature 100 °C
 0.0000100 ohm-cm
@Temperature 150 °C
 0.0000101 ohm-cm
@Temperature 200 °C
 0.0000104 ohm-cm
@Temperature 250 °C
 0.0000110 ohm-cm
@Temperature 300 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.0 µm/m-°C
@Temperature 30.0 - 50.0 °C
 14.5 µm/m-°C
@Temperature 30.0 - 100 °C
 15.0 µm/m-°C
@Temperature 30.0 - 150 °C
 15.5 µm/m-°C
@Temperature 30.0 - 200 °C
 15.5 µm/m-°C
@Temperature 30.0 - 250 °C
 15.5 µm/m-°C
@Temperature 30.0 - 300 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
 0.470 J/g-°C
@Temperature 50.0 °C
 0.480 J/g-°C
@Temperature 100 °C
 0.495 J/g-°C
@Temperature 150 °C
 0.505 J/g-°C
@Temperature 200 °C
 0.515 J/g-°C
@Temperature 250 °C
 0.525 J/g-°C
@Temperature 300 °C
Thermal Conductivity 11.0 W/m-K
@Temperature 20.0 °C
 11.0 W/m-K
@Temperature 50.0 °C
 12.0 W/m-K
@Temperature 100 °C
 13.0 W/m-K
@Temperature 150 °C
 14.0 W/m-K
@Temperature 200 °C
 15.0 W/m-K
@Temperature 250 °C
 16.0 W/m-K
@Temperature 300 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.020 %
Chromium, Cr 27 %
Copper, Cu 1.0 %
Manganese, Mn <= 2.0 %
Molybdenum, Mo 3.5 %
Nickel, Ni 31 %
Phosphorus, P <= 0.025 %
Silicon, Si <= 0.60 %
Sulfur, S <= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Sanicro 28 Seamless tube and pipe
Special Metals INCONEL® Alloy 718
Sandvik Sanicro 28 Bar Steel
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications
Overview of materials for 7000 Series Aluminum Alloy

NSANDV5249 / 199813

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.