MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phosphorous, P, White
Categories: Pure Element

Key Words: Phosphorus
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.823 g/cc0.06586 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 30.9737630.9737630.973761 - 1995
Atomic Number 1515
X-ray Absorption Edge 5.7866 Å5.7866 ÅK
 81.02 Å81.02 ÅLI
 96.843 Å96.843 ÅLII
 96.843 Å96.843 ÅLIII
Critical Temperature 721 °C1330 °F
Electronegativity 2.192.19Pauling
Ionic Radius 0.350 Å0.350 ÅCrystal Ionic Radius for Valence +5
 0.440 Å0.440 ÅCrystal Ionic Radius for Valence +3
 2.12 Å2.12 ÅCrystal Ionic Radius for Valence -3
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.769 J/g-°C0.184 BTU/lb-°F
Melting Point 44.15 °C111.5 °FTriple Point
Boiling Point 280.5 °C536.9 °F
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 100 %100 %
 
Descriptive Properties
AppearanceColorless, Waxy cubic crystals
CAS Number7723-14-0
 7723-14-0

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phosphorous, P, Red
Phosphorous, P, Black
Gallium, Ga
Graphite, Carbon, C
Arsenic, As

AMEP00 / 3711

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.