MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dow Dow™ DMDD-3220 NT 7 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: Dow DMDD-3220 NT 7 HDPE is produced via UNIPOL™ Processing Technology from Dow and is intended for rotational and injection molding is specifically designed for applications requiring excellent processability and aesthetics combined with low warpage and good mechanical properties. Processing and Stabilization: Dow DPDA-3220 NT 7 HDPE is fully heat and UV stabilized resulting in a wide processing latitude, good color retention and long life expectancy.
  • Rotational molding or injection molding
  • For Large Agricultural Tanks, Intermediate Bulk Containers, Potable Water, Chemical Tanks and Industrial Products
  • Excellent impact strength, stress crack resistance and processability
Complies with: US FDA 21 CFR 177.1520©3.1a; Canadian HPFB No Objection; EU No 10/2011. Consult the regulations for complete details.

Availability: Asia Pacific; Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520©3.1a; Canadian HPFB No Objection; EU No 10/2011

Form: Pellets

Processing Method: Injection Molding; Rotational Molding

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ASTM D792
ESCR 100% Igepal®  >= 743 hour
@Temperature 50.0 °C
>= 743 hour
@Temperature 122 °F
F50, Plaque molded and tested in accordance with ASTM D4976; ASTM D1693A
 >= 1000 hour
@Temperature 50.0 °C
>= 1000 hour
@Temperature 122 °F
F50, Plaque molded and tested in accordance with ASTM D4976; ASTM D1693B
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 21.4 MPa3100 psiPlaque molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Break 710 %710 %Plaque molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Yield 12 %12 %Plaque molded and tested in accordance with ASTM D4976; ASTM D638
Flexural Modulus 0.738 GPa107 ksi1% Secant, Plaque molded and tested in accordance with ASTM D4976; ASTM D790B
 0.986 GPa143 ksiPlaque molded and tested in accordance with ASTM D4976; ASTM D790B
Impact Test >= 271 J
@Thickness 6.35 mm,
Temperature -40.0 °C
>= 200 ft-lb
@Thickness 0.250 in,
Temperature -40.0 °F
Rotational Molded
 
Thermal PropertiesMetricEnglishComments
Melting Point 127 °C261 °F
Deflection Temperature at 0.46 MPa (66 psi) 55.6 °C132 °FUnannealed, Plaque molded and tested in accordance with ASTM D4976; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 41.7 °C107 °FUnannealed, Plaque molded and tested in accordance with ASTM D4976; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF459 / 311152

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.