Description: AKROMID B3 GF 40 black (3383) is a 40% glass fiber reinforced polyamide 6 with high rigidity and strength. Applications are mainly components in mechanical engineering and in the automotive industry. Features: - High Stiffness
- High Strength
Uses:- Automotive Application
- Engineering Parts