MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP Radel R-7300 Polyphenyl Sulfone (PPSU); Flame Retardant
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Aircraft interior grade material. Complies with AITM 2.0007 & BSS 7238 test methods for Smoke Density, <200 Ds@4min in the flaming mode. Complies with AITM 3.0005 & BSS 7239 for Toxic Gas Emission at 4 minutes. Complies with OSU 55/55 Heat Release (2 Minute Test) per FAR 25.853.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.36 g/ccASTM D 792
Water Absorption 0.30 %
@Time 86400 sec
ASTM D 570
Melt Flow 16 g/10 min
@Load 2.16 kg
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 11000 psiASTM D 638
Elongation at Break 40 %ASTM D 638
Tensile Modulus 400 ksiASTM D 638
Flexural Strength 16000 psiASTM D 790
Flexural Modulus 400 ksiASTM D 790
Izod Impact, Notched 1.50 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
ASTM D 4812
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 360 °FASTM D 648
Flame Spread 1.00 in/min
@Thickness 1.50 mm
Aerospace; FMVSS 302
 
Processing PropertiesOriginal ValueComments
Melt Temperature 650 - 710 °F
Mold Temperature 275 - 350 °F
Drying Temperature 300 °F
@Time 21600 sec
Moisture Content 0.040 %
Dew Point -25.0 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP Radel R-7625 Polyphenyl Sulfone (PPSU); Flame Retardant
RTP Company RTP Radel R-7700 Polyphenyl Sulfone (PPSU); Flame Retardant
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)
Westlake Plastics Radel® R 4400 Polyphenylsulfone For Medical Applications
Westlake Plastics Radel® R Polyphenylsulfone

PQZRA32271 / 206051

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.