MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Shandong Dongyue Polymer TFP Tetrafluoropropanol
Categories: Fluid

Material Notes: Usage: TFP is widely used on medicine, agrichemical, dyestuff and intermediate of fine chemical such as the color agent of photography, textile finishing agent, fluoropolymer assistant ingredient, detergent for electronic product etc. TFP is an excellent replacement for Freon detergent for its environment-friendly property.

Storage: Closed store in shadow and cool place.

Properties: TFP is colorless and transparent liquid, and nonflammable, low toxicity, noncorrosivity and excellent lubricity with fragrance like alcohol. TFP is miscible with many organic solvents.

Molecular Formula: C3F4H4O

Structural Formula: HCF2CF2CH5OH

Information provided by Shandong Dongyue Polymer Material Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.485 g/cc
@Temperature 20.0 °C
1.485 g/cc
@Temperature 68.0 °F
pH 6.0 - 8.06.0 - 8.0
Molecular Weight 132 g/mol132 g/mol
Vapor Pressure 9.00 bar6750 torr
 
Thermal PropertiesMetricEnglishComments
Melting Point -15.0 °C5.00 °F
Boiling Point 109 °C228 °F
Flash Point 47.5 °C118 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.32
@Temperature 20.0 °C
1.32
@Temperature 68.0 °F
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.00020 %<= 0.00020 %
 
Descriptive Properties
Purity (%)90

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSHADP20 / 103671

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.