MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC LNP™ STAT-LOY™ Compound D3000IEU6 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-LOY D3000IEU6 Compound is a static dissipative Polycarbonate Copolymer based compound that has been designed towards ATEX compliant applications. The material has an optimized balance between surface resistivity and impact strength retention after hydro aging, and has excellent low temperature impact. The material is available in a wide range of dark and light colors, including UV stabilization.

Features: Electrostatic discharge (ESD),Hydrolytic Stability,Enhanced Low Temperature Impact,Enhanced Ductility,Easy Flow,Amorphous,General Purpose,Custom Color,Appearance & Durability,Dielectrics,Thin Wall,Colorable,Color Stability,Weatherable,UV Resistant,High Impact Resistance,High Flow,Heat Stabilized,Good Moldability,Good Mold Release,Ductile,Antistatic

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccASTM D792
Density 1.16 g/cc0.0419 lb/in³ISO 1183
Water Absorption  0.70 %
@Time 86400 sec
0.70 %
@Time 24.0 hour
ASTM D570
 0.70 %
@Time 86400 sec
0.70 %
@Time 24.0 hour
ISO 62-1
Moisture Absorption 0.0300 %0.0300 %Injection Molding
 0.150 %0.150 %23°C/50% RH/24 hrs; ISO 62-4
Moisture Absorption at Equilibrium 0.30 %0.30 %23°C/50% RH; ISO 62-4
Water Absorption at Saturation 3.5 %3.5 %ASTM D570
 3.5 %3.5 %ISO 62-1
Viscosity  5.0 cP
@Load 2.16 kg,
Temperature 250 °C
5.0 cP
@Load 4.76 lb,
Temperature 482 °F
MVR cc/10 min; ISO 1133
 15 cP
@Load 5.00 kg,
Temperature 250 °C
15 cP
@Load 11.0 lb,
Temperature 482 °F
MVR cc/10 min; ISO 1133
 23 cP
@Load 5.00 kg,
Temperature 260 °C
23 cP
@Load 11.0 lb,
Temperature 500 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inSABIC method
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inSABIC method
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 250 °C
15 g/10 min
@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 78.0 MPa11300 psiH358/30; ISO 2039-1
Tensile Strength, Yield 45.0 MPa6530 psi50 mm/min; ASTM D638
 45.0 MPa6530 psi50 mm/min; ISO 527
Elongation at Break >= 60 %>= 60 %50 mm/min; ASTM D638
 >= 60 %>= 60 %50 mm/min; ASTM D638
 >= 60 %>= 60 %50 mm/min; ISO 527
 >= 60 %>= 60 %50 mm/min; ISO 527
Elongation at Yield 5.5 %5.5 %50 mm/min; ASTM D638
 5.5 %5.5 %50 mm/min; ISO 527
Tensile Modulus 1.75 GPa254 ksi50 mm/min; ASTM D638
 1.75 GPa254 ksi1 mm/min; ISO 527
Flexural Strength 70.0 MPa10200 psi1.3 mm/min, 50 mm span; ASTM D790
 70.0 MPa10200 psi2 mm/min; ISO 178
Flexural Modulus 1.825 GPa264.7 ksi2 mm/min; ISO 178
 1.90 GPa276 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 850 J627 ft-lbASTM D256
 750 J
@Temperature -30.0 °C
553 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched NBNBASTM D4812
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ASTM D4812
Izod Impact, Notched (ISO) 60.0 kJ/m²28.6 ft-lb/in²80*10*4; ISO 180/1A
 65.0 kJ/m²30.9 ft-lb/in²80*10*3; ISO 180/1A
 60.0 kJ/m²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
 65.0 kJ/m²
@Temperature -30.0 °C
30.9 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*3; ISO 180/1U
 NBNB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBNBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 6.00 J/cm²28.6 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 35.0 J25.8 ft-lbpeak; ASTM D3763
 40.0 J29.5 ft-lbASTM D3763
 35.0 J
@Temperature -30.0 °C
25.8 ft-lb
@Temperature -22.0 °F
peak; ASTM D3763
 40.0 J
@Temperature -30.0 °C
29.5 ft-lb
@Temperature -22.0 °F
ASTM D3763
Impact Test 55.0 J40.6 ft-lbMulti-Axial Instrumented Impact Energy @ peak, 23°C; ISO 6603-2
 55.0 J40.6 ft-lbMulti-Axial Instrumented Impact Energy @ peak, -30°C; ISO 6603-2
 65.0 J47.9 ft-lbMulti-Axial Instrumented Impact Total Energy, 23°C; ISO 6603-2
 65.0 J47.9 ft-lbMulti-Axial Instrumented Impact Total Energy, -30°C; ISO 6603-2
Dart Drop Test 408000 g900 lbASTM D3763
 489600 g
@Temperature -30.0 °C
1080 lb
@Temperature -22.0 °F
ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+9 - 1.00e+11 ohm1.00e+9 - 1.00e+11 ohmASTM D257
 1.00e+9 - 1.00e+11 ohm1.00e+9 - 1.00e+11 ohmROA; IEC 60093
Static Decay <= 0.010 sec<= 0.010 sec5000V to <50V; FTMS101B
Dielectric Constant 2.73
@Frequency 6.00e+10 - 9.00e+10 Hz
2.73
@Frequency 6.00e+10 - 9.00e+10 Hz
Dissipation Factor 0.022
@Frequency 6.00e+10 - 9.00e+10 Hz
0.022
@Frequency 6.00e+10 - 9.00e+10 Hz
Comparative Tracking Index 175 V175 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  85.0 µm/m-°C
@Temperature 23.0 - 50.0 °C
47.2 µin/in-°F
@Temperature 73.4 - 122 °F
ASTM E831
 85.0 µm/m-°C
@Temperature 23.0 - 50.0 °C
47.2 µin/in-°F
@Temperature 73.4 - 122 °F
ISO 11359-2
CTE, linear, Transverse to Flow  110 µm/m-°C
@Temperature 23.0 - 50.0 °C
61.1 µin/in-°F
@Temperature 73.4 - 122 °F
ASTM E831
 110 µm/m-°C
@Temperature 23.0 - 50.0 °C
61.1 µin/in-°F
@Temperature 73.4 - 122 °F
ISO 11359-2
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 123 °C253 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 123 °C
@Thickness 3.20 mm
253 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 105 °C
@Thickness 3.20 mm
221 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 123 °C253 °FRate B/120; ASTM D1525
 123 °C253 °FRate B/50; ASTM D1525
 123 °C253 °FRate B/120; ISO 306
 123 °C253 °FRate B/50; ISO 306
 137 °C279 °FRate A/50; ISO 306
 138 °C280 °FRate A/120; ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 240 - 260 °C464 - 500 °F
Zone 2 230 - 250 °C446 - 482 °F
Zone 3 240 - 260 °C464 - 500 °F
Melt Temperature 240 - 260 °C464 - 500 °FInjection Molding
Mold Temperature 50.0 - 90.0 °C122 - 194 °F
Drying Temperature 80.0 - 95.0 °C176 - 203 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
 
Descriptive Properties
Screw speed (Circumferential speed)0.15-0.2 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81410 / 289357

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.