MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Keltan® Eco 5470 Ethylene-Propylene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Highly crystalline ethylene-propylene rubber with medium ENB (ethylidene norbornene) content and a medium Mooney viscosity. This product is fully made with ethylene from sugar cane, which can be tested with ASTM D6866. The combination of a highly crystalline structure with a narrow molecular weight distribution and medium viscosity provides an extremely robust polymer with good processing characteristics. Due to the high crystallinity of the grade is broadly applicable e.g. for solid sealing systems, hoses, mechanical goods and low voltage cable applications.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.860 g/cc
Mooney Viscosity 55
@Temperature 125 °C
(1+4); ISO 289
Storage Temperature >= 30.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 36.0 Month
 
Descriptive Properties
Content4.6 percentENB, ASTM D6047
 70 percentEthylene, ASTM D3900

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lanxess Keltan® 9950C Ethylene-Propylene Rubber
Lanxess Keltan® 5465Q Ethylene-Propylene Rubber
Lanxess Keltan® 5470Q Ethylene-Propylene Rubber
Lanxess Keltan® 6160D Ethylene-Propylene Rubber
Lanxess Keltan® 7752C Ethylene-Propylene Rubber

PLANY8602 / 208995

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.